PHYSICAL SPECIFICATIONS
| PROPERTY |
TEST METHOD |
METRIC |
ENGLISH |
| THICKNESS |
ASTM D-751 |
1 MM NOMINAL |
40 MIL NOMINAL |
| TEAR STRENGH, LBS |
ASTM D-751, TONGUE METHOD, 8"X8" SAMPLE |
578 X 489 N |
130 X 110 LBS |
| BREAKING STRENGTH |
ASTM D-751 |
1,935 X 1,557 N |
435 X 350 LBS |
| EMMAQUA EXPOSURE |
ASTM E938, DESERT SUN |
>256,307 MJ/m² |
6.9 MILLION LANGLEYS |
| ELONGATION |
ASTM D-751 |
35% |
35% |
| DIMMENSION STABILITY, % OF CHANGE |
ASTM D-1204 |
<0.1% |
<0.1% |
| LOW TEMPERATURE FLEXIBILITY |
ASTM D-2136 ⅛" MANDREL |
NO CRACKS -40 DEGREES F |
NO CRACKS -40 DEGREES F |
| DYNAMIC IMPACT |
FED. STD. 101B METHOD B |
1,557 N |
350 LBS |
| WATER VAPOR TRANSMISSION |
ASTM E96 PROCEDURE B METHOD A |
0.130 g/h/m² |
.25 US PERMS |
| ACCELERATED WEATHERING |
CARBON ARC 6,000 HRS |
NO CRACKING, CRAZING, OR BLISTERING |
| ACCELERATED WEATHERING UVB-313 LAMP @ 80 DEGREES C |
ASTM G-53 88 2,000 HRS |
NO CRACKING, CRAZING, OR BLISTERING |
| FACTORY MUTUAL RESEARCH |
FM 4450/4470 |
CLASS: 1-60, 1-90, 1-105, 1-150, 1-210 |
| UNDERWRITERS LABORATORY |
UL-790 UL 1897 |
CLASS: A, B OR C |